Hardness Conversion Calculator
Convert between Rockwell C, Rockwell B, Rockwell A, Brinell, Vickers, Knoop and Shore hardness using ASTM E140 / ISO 18265 correlations. Includes material presets and a live conversion table.
Understanding Hardness Conversion
Hardness is a measure of a material's resistance to localised plastic deformation. Several test methods exist — Rockwell, Brinell, Vickers, Knoop and Shore — and each produces a number on its own scale. Hardness conversion is the empirical process of estimating the equivalent value on another scale, usually following ASTM E140 or ISO 18265.
Conversions are not exact physical laws: they are statistical correlations derived from large test programmes on specific material families. For specification and acceptance testing, always measure on the scale required by the drawing or standard.
Key relations used in this calculator (steel baseline):
HV ≈ 1.05 · HB + 5
HRC ≈ −29.8 + 0.108 · HV − 4.83×10⁻⁵ · HV² (valid HV ≥ 240)
HK ≈ 0.985 · HV
HS ≈ 0.05 · HV + 8
σB [MPa] ≈ 3.5 · HB
How the Hardness Conversion Calculator Works
Enter a hardness value and select its scale. The calculator then:
- Converts the input to a Vickers HV anchor value using scale-specific inverse relations.
- Propagates HV to HB, HRC, HRB, HRA, HK and HS using the ASTM E140 / ISO 18265 correlations.
- Applies a material-family correction for non-ferrous metals (aluminium, copper, brass).
- Estimates tensile strength from HB for steels.
- Builds a conversion table around your value and highlights the closest row.
- Draws a conversion curve (HV vs HRC) with your operating point marked.
Scales Supported
- Vickers (HV) — diamond pyramid, load 1–100 kgf. Universal scale, good for hard and soft materials.
- Brinell (HB / HBW) — 10 mm tungsten-carbide ball, typically 3000 kgf. Good for castings and forgings.
- Rockwell C (HRC) — diamond cone, 150 kgf. The standard for hardened steel; unreliable below ≈ HRC 20.
- Rockwell B (HRB) — 1/16″ steel ball, 100 kgf. Used for soft steels and non-ferrous metals.
- Rockwell A (HRA) — diamond cone, 60 kgf. Used for very hard materials and thin specimens.
- Knoop (HK) — rhombic pyramid. Used for coatings, thin layers and brittle materials.
- Shore scleroscope (HS) — dynamic rebound test. Portable field check for large rolls and castings.
Why HRC Has a Lower Limit
The Rockwell C test uses a diamond cone and a 150 kgf major load. Below about HRC 20 (HB ≈ 235, HV ≈ 240), the indenter penetrates deeply and the dial reading scatters. Softer materials should be tested on Rockwell B (steel ball, 100 kgf) or another scale. This calculator shows a dash for HRC when the value is outside its reliable range.
Ferrous vs Non-Ferrous Conversions
Steels and cast irons of all conditions — annealed, normalised, quenched and tempered or fully hardened — lie on a single conversion curve spanning roughly HV 80 to HV 1000. Aluminium, copper and brass, however, are physically distinct: at the same Vickers hardness they read 20–25 HRB points apart. This calculator applies a material-family shift so the HRB output is appropriate for the selected alloy family.
Assumptions and Limitations
- Conversions are approximate and material-specific; they are not a substitute for direct measurement.
- The steel baseline uses ASTM E140 / ISO 18265 mean curves; individual heats may deviate by ±5 %.
- Tensile-strength estimates are rough (±15 %) and valid for steels only.
- Shore (HS) and Knoop (HK) correlations have wider scatter (±15 %) than HV–HB–HRC relations.
- Conversions assume the material is homogeneous and the indentation is well formed; surface preparation and test load matter.
Use these results as a learning aid or for preliminary cross-checking. Always verify against the governing standard and, where required, measure on the specified scale.
❓ Hardness Conversion Calculator FAQ
How accurate is a hardness conversion?
Hardness conversions are empirical correlations, not physical laws. ASTM E140 and ISO 18265 give approximate equivalents, typically accurate to within ±5 % for steels. For specification or acceptance testing, always measure on the scale required by the drawing or standard.
Why does HRC show a dash below about HRC 20?
The Rockwell C scale uses a 150 kgf load on a diamond cone and is designed for hardened steel. Below roughly HRC 20 (HB 235, HV 240) the indenter sits near the bottom of the dial and readings scatter. Softer materials should be tested on Rockwell B (HRB) or another scale.
Can I convert HRC directly to HV?
Yes, but only approximately and only above about HV 240. A common ASTM E140 fit is HRC ≈ −29.8 + 0.108·HV − 4.83×10⁻⁵·HV². The conversion is non-linear: HRC increases quickly at high hardness but flattens at low hardness.
What is the difference between HB and HBW?
HB is the generic Brinell hardness symbol. HBW denotes a Brinell test using a tungsten carbide ball indenter (the modern standard). Older tables may use HBS for hardened steel balls. For most engineering purposes HB and HBW values are equivalent.
Does material affect the conversion?
Yes. Steels and cast irons share one conversion curve, but aluminium, copper and brass each follow distinct curves. At the same Vickers hardness, brass, copper and aluminium can differ by 20–25 HRB points. Always select the correct material family.
What is Knoop hardness?
Knoop hardness (HK) uses a rhombic pyramidal diamond indenter and is often used for thin specimens, coatings and brittle materials. For steels it is approximately HK ≈ 0.985·HV, but the ratio varies with material and load.
What is Shore hardness (HS)?
Shore scleroscope hardness is a dynamic rebound test, different from the Shore A/D durometer used for polymers. For metals, an empirical relation is HS ≈ 0.05·HV + 8, accurate to about ±15 %. It is mainly used for field checks on large rolls and castings.
Can I estimate tensile strength from hardness?
Yes, approximately. For steels, σ_B ≈ 3.5 × HB in MPa (or σ_B ≈ 500 × HB in psi). This is a rough rule of thumb with ±15 % scatter and should not replace a tensile test for design or certification.